Universal Wire Works 17-22ASVM (AMS 6458) Low Alloy Steel Welding Wire
Subcategory: Low Alloy Steel; Metal
Material Notes: Iron content is calculated as remainder. Alloy 17-22ASVM is a controlled chemistry vacuum melted filler metal of premium quality. This alloy is primarily used with the gas tungsten arc and gas metal arc processes for low alloy steels of similar composition where the weld metal is required to have strength comparable to that of the parent metal. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|