Universal Wire Works 502 (AMS 6466) Low Alloy Steel Welding Wire
Subcategory: Low Alloy Steel; Metal
Material Notes: Iron content is calculated as remainder. Alloy 502 is a 5% chromium, 0.5% molybdenum alloy for use as filler metal for welding low-alloy steels where response to heat treatment is required in weld. Used extensively with the gas metal arc, gas tungsten arc and submerged arc welding processes. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |