Universal Wire Works HP9-4-20 (AMS 6468) Low Alloy Steel Welding Wire
Subcategory: Low Alloy Steel; Metal
Material Notes: Iron content is calculated as remainder. Alloy HP9-4-20 is a premium quality low alloy steel filler metal for use with the gas tungsten arc and gas metal arc welding processes. Alloy HP9-4-20 is designed to weld those low-alloy steels having compositions similar to that of this wire and requiring a combination of high strength and high notch toughness without the need for post-weld heat treatment. Information provided by Universal Wire Works for their line of welding wire and filler metal.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|