Universal Wire Works No. 21 Cobalt Alloy Welding Wire

 

Subcategory: Superalloy; Nonferrous Metal; Cobalt Alloy; Cobalt Base

Material Notes:
Cobalt content is calculated as remainder.

Universal No. 21 is a cobalt-chromium-molybdenum alloy designed for covered electrode, TIG, MIG, hard surfacing applications. The work-hardening characteristics, high ductility properties, excellent resistance to impact and metal to metal wear suit Universal 21 to severe applications where a work-hardening material is desired (as welded Rc 20; work hardened Rc 40 - 43).

Universal 21 applications include: high temperature valves, high pressure valves, hot punches crushing knives, drop forging dies, tap hole augers, pump shafts and sleeves, press dies, vapor tight valve seats.

This alloy has the best impact resistance of the cobalt based alloys. Alloy 21 work hardens in service, has excellent erosion, corrosion and metal to metal wear resistance. Deposits exhibit effective hardness and a good cutting edge at high temperatures. On thick overlays Alloy 21 can be used as a buildup prior to depositing a higher hardness alloy.

Machinability: Use carbide tools.

Information provided by Universal Wire Works for their line of welding wire and filler metal.

Available Properties
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。