COLMONOY® 5 - Hard-Surfacing Alloy Containing Wear-Resistant Chromium Borides and Carbides
Subcategory: Metal Matrix Composite; Nickel Alloy; Nonferrous Metal; Nickel Base
Close Analogs: Nickel content calculated as balance.
Material Notes: Description: Contains wear-resistant chromium borides and carbides. Has greater ductility, better impact resistance and workability than Colmonoy No. 6 Finished with carbide tools and grinding. Applications: For wear rings, plungers, dies. Method of Application: Oxyacetylene, DC Electric Arc, GTAW, Spraywelder Information provided by Wall Colmonoy Corporation.
| Available Properties |
- Density
- Hardness, Rockwell C
- Melt Temperature
|
|
|
|