COLMONOY® 23A & 24 - Nickel Alloy With Tungsten Carbide
Subcategory: Metal Matrix Composite; Nickel Alloy; Tungsten Alloy; Nonferrous Metal; Nickel Base
Close Analogs: Nickel content calculated as balance.
Material Notes: Description and Application: Used to repair blow holes, flaws, chips, and cracks in cast iron parts. No. 23A works best in repairing surface flaws, No. 24 is recommended for working on edges or corners. Finished by grinding or filing.Method of Application: Fusewelder Information provided by Wall Colmonoy Corporation.
| Available Properties |
- Density
- Hardness, Rockwell C
- Melt Temperature
|
|
|
|
| Property Data |