COLMONOY® 84 - Nickel-Based Alternative to Cobalt Surfacing Alloys
Subcategory: Metal Matrix Composite; Nickel Alloy; Tungsten Alloy; Nonferrous Metal; Nickel Base
Close Analogs: Nickel content calculated as balance.
Material Notes: Description and Application: A nickel-based alternative to cobalt surfacing alloys, for service temperatures up to 1500°F. Boron and silicon content provide better weldability at lower application temperatures.Method of Application: Spraywelder, Fusewelder, PTA Information provided by Wall Colmonoy Corporation.
| Available Properties |
- Density
- Hardness, Rockwell C
- Melt Temperature
|
|
|
|
| Property Data |