COLMONOY® 88 Hard-Surfacing Alloy
Subcategory: Metal Matrix Composite; Nickel Alloy; Tungsten Alloy; Nonferrous Metal; Nickel Base
Close Analogs: Nickel content calculated as balance.
Material Notes: Description: Colmonoy 88 is a unique alloy containing fine, multiple hard phases which are uniformly distributed throughout a Ni-Cr-B matrix. These hard phases, comprised of complex bi- and tri-metallic borides and carbides, are precipitated during manufacturing, and are therefore an inherent part of the microstructure and not added externally as in conventional composite powders. The hard phases, remain uniformly distributed shipping, spraying and fusing to ensure consistent performance throughout the coating. They are an intimate part of the matrix and will not erode prematurely. Their fine size (5-10 microns) contributes to better finishing characteristics. The hard phases, along with the high-hardness Ni-Cr-B matrix, resist extreme abrasion and corrosion.Method of Application: Spraywelder, HVOF, Fusewelder, PTA Applications: Colmonoy 88 has proved successful in increasing the service life of glass mold plungers, where the alloy withstands wear from hot (1800°F), extremely abrasive, molten silica. Other applications include: pump plungers and sleeves, valve seats, thermowells, centrifuges, plastics processing screws and barrels, wire drawing capstans, and catalytic cracker components. Information provided by Wall Colmonoy Corporation.
| Available Properties |
- Density
- Hardness, Rockwell C
- Solidus
- Liquidus
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|