COLTUNG 1 - Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide
Subcategory: Metal Matrix Composite; Nickel Alloy; Tungsten Alloy; Nonferrous Metal; Nickel Base; Cobalt Alloy
Close Analogs: Nickel content calculated as balance.
Material Notes: Description and Application: A nickel-chromium-boron matrix alloy rich in chromium boride is used to hold extremely hard tungsten-carbide particles. Produces rod-welded deposits with same chemistry as spray-applied Colmonoy® Nos. 75 or 705. Finished by grinding. Information provided by Wall Colmonoy Corporation.
| Available Properties |
- Density
- Hardness, Rockwell C
- Melt Temperature
|
|
|
|
| Property Data |