WALLEX 40 - Cobalt-Nickel Alloy
Subcategory: Metal Matrix Composite; Nickel Alloy; Tungsten Alloy; Nonferrous Metal; Nickel Base; Cobalt Base
Close Analogs: Cobalt content calculated as balance.
Material Notes: Description: A cobalt-nickel alloy powder that forms deposits similar to those of Wallex 50, but softer. Finished with carbide tools and grinding.Method of Application: Spraywelder, Fusewelder, PTA, HVOF Information provided by Wall Colmonoy Corporation.
| Available Properties |
- Density
- Hardness, Rockwell C
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|