Wieland Auropal 2 Casting Alloy
Subcategory: Silver Alloy; Precious Metal; Gold Alloy; Metal
Close Analogs: Dental
Key Words: EN ISO 8891
Material Notes: Gold-silver casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneering
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Processing Temperature
- Melt Temperature
- Casting Temperature
- Color
|
|
|
|
| Property Data |