Wieland REFLEX® Ceramic Veneering
Close Analogs: Dental
Material Notes: Innovative veneering ceramic with extremely smooth, homogeneous and plaque resistant surface. Also, it is gingiva and antagonist friendly as well as chairside polishable. The opalescence remains stable during multiple firingsApplications: ceramic veneering
| Available Properties |
- CTE, linear 500°C
- Processing Temperature
|
|
|
|