Wieland Wilaform Gold 1403
Subcategory: Precious Metal; Nonferrous Metal; Gold Alloy
Close Analogs: Dental
Material Notes: Hard yellow gold alloy. Universally applicable in decoration production. Since it does not posses a very fine-grained structure it is used frequently for chainsApplications: casting, chains, laminar decoration
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Elongation at Break
- Processing Temperature
- Casting Temperature
- Color
- Fusion Interval °C
|
|
|
|