Williams Advanced Alloys Solder Alloy WS96
Subcategory: Lead Alloy; Solder/Braze Alloy
Material Notes: All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring and wire. Custom shapes can also be manufactured using our state-of-the-art design and fabrication equipment.Information provided by Williams Advanced Alloys
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Electrical Resistivity
- CTE, linear 20°C
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |