Hardwire, LLC 3SX Cord

 

Subcategory: Brass; High Carbon Steel; Metal

Material Notes:
Description: The 3SX Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 3SX cord is used where balanced compressive and tensile strengths are required as well as better handling characteristics than the 3S. The 3SX wire cord is made by twisting three identical wire filaments (All filaments are 0.0189 in diameter) together at a longer than usual lay length and then over-wrapping the bundle with a single filament. The result is a cord with lower twist angles and straighter filaments that is the basis for the increased compressive strengths.

Characteristics:

  • 3SX tapes have the highest compressive strengths of all Hardwire tapes and tend to match or exceed the tensile properties.
  • Increased mechanical bonding in resins.
  • Better interlaminar shear resistance.
  • The cords do not bloom in failure modes during compression or tension.
  • Laminates exhibit steel like characteristics with high ductility and extreme deflection capability.
  • Very high flexural strength as well as ductile failure modes (laminates tend to bend – not break).
  • The best tape for bending angles and can be done in standard sheet metal breaks.
  • Very boardy feel – excellent for flat surfaces but still conformable enough for curved structures.
  • Better handling characteristics and cutability than 3S tapes.

All information provided by Hardwire, LLC.

Available Properties
  • Tensile Strength @ Break
  • Elongation at Break
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。