Hardwire, LLC 12x Cord

 

Subcategory: Brass; High Carbon Steel; Metal

Material Notes:
Description: The 12X Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 12X wire cord is used where the traits of high tensile strain, excellent conformability, great looks and bond-ability to very high viscosity resins are required. The 12X wire cord is made by twisting two different individual wire diameters together in 12 strands and then over twisting 1 wire around the bundle (3 @ 0.00866 in and 9 @ 0.00784, plus wrap). The result is very flexible wire cord with great tensile strain capability.

Characteristics:

  • The 12X cord is the most flexible cord and should be used for more complex structures.
  • The over-wrap wire creates a mechanical lock with the resin system and with the other 12X wires it interacts with.
  • The over-wrap wire also creates a perfect standoff for adhesive bonding. This wire type is preferred in applications where the wire layer is in place on a preexisting substrate and resin is rolled on to the surface. In this case the over wrap wire creates a small stand off from the surface allowing for the perfect amount of adhesive resin to penetrate behind the wire layer and wet the original preexisting substrate being reinforced.
  • The cord bonds to highly viscous resin systems like cementitious systems or highly filled thermosets or traditional thermoplastics. In these cases the over wrap wire functions the way threads act on a screw, forming a strong mechanical interlock with the resin being used.
  • Under tension loads the over wrap wire works to tighten down on the other 12 wires thus optimizing the composite action of the wire cord and evenly sharing the tensile load between all the individual wires contained in the cord structure.
  • The 12X cord is the best looking for architectural applications. The complex geometry of the 12X cord works to diffract light and add engineering appeal to your structure.

All information provided by Hardwire, LLC.

Available Properties
  • Tensile Strength @ Break
  • Elongation at Break
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。