MMCC Al/SiC Particulate Aluminum Matrix Composite
Subcategory: Metal Matrix Composite; Carbide; Aluminum Alloy; Nonferrous Metal
Key Words: Metal Matrix Cast Composites, Metal Matrix Composites; Aluminium; Silicon Carbide
Material Notes: Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform. Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Fracture Toughness
- CTE, linear 20°C
- Thermal Conductivity
|
|
|
|
| Property Data |