Overview - Acetal Homopolymer, Glass Fiber Reinforced
Subcategory: Acetal; Thermoplastic; Polymer
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: POM, Polyoxymethylene; Polyformaldehyde; Polyacetal; Plastics, Polymers
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Rockwell M
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Poissons Ratio
- Fatigue Strength
- Shear Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Tensile Impact Strength
- Coefficient of Friction
- Taber Abrasion, mg/1000 Cycles
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Processing Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|