Overview - Acrylic, Cast
Subcategory: Acrylic; Thermoplastic
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate; Plastics, Polymers
Available Properties |
- Density
- Water Absorption
- Water Absorption at Saturation
- Hardness, Barcol
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Minimum Service Temperature, Air
- Glass Temperature
- Refractive Index
- Haze
- Transmission, Visible
- Processing Temperature
|
|
|
|
Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|