Overview - Epoxy Encapsulant, Unreinforced
Subcategory: Epoxy; Thermoset; Polymer
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: Plastics, Polymers
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Spiral Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Thermal Conductivity
- Maximum Service Temperature, Air
- Glass Temperature
- Flammability, UL94
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|