Overview - Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Subcategory: Fluoropolymer; Thermoplastic; PTFE; Polymer
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: Fluoropolymer; Plastics, Polymers
| Available Properties |
- Density
- Apparent Bulk Density
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Compressive Modulus
- Izod Impact, Notched
- Coefficient of Friction
- Coefficient of Friction, Static
- K Factor (Wear Factor)
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|