Overview - Fluorinated Ethylene Propylene (FEP), Molded/Extruded
Subcategory: Fluoropolymer; Thermoplastic; FEP
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: Plastics, Polymers
| Available Properties |
- Density
- Water Absorption
- Moisture Vapor Transmission
- Oxygen Transmission
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Compressive Yield Strength
- Poissons Ratio
- Fatigue Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- Coefficient of Friction
- Limiting Pressure Velocity
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- CTE, linear 20°C
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Oxygen Index
- Refractive Index
- Transmission, Visible
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|