Overview - Nylon 66, Film
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: Polyamide 66; PA66; PA 66; Polyamide 6/6; Polyamide 6,6; Nylon 6/6; Nylon 6,6; Plastics, Polymers
| Available Properties |
- Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Coefficient of Friction
- Dart Drop Test
- Haze
- Gloss
|
|
|
|
| Property Data |