Overview - Phenolic, Novolac, Impact Grade, Filled
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: Plastics, Polymers; Phenol-Formaldehyde
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Izod Impact, Notched
- Charpy Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|