Overview - PET, Polyethylene terephthalate, 20% Titanium Dioxide Filler
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic; Polymer
Key Words: Polyester; Plastics, Polymers
Material Notes: Polymer properties are subject to a wide variation, depending on the grade specified.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
|
|
|
|