Overview - Ethylene Vinyl Acetate Copolymer (EVA), Sheet Extrusion Grade
Subcategory: Ethylene Vinyl Acetate; Thermoplastic; Polymer
Key Words: Plastics, Polymers
Material Notes: Polymer properties are subject to a wide variation, depending on the grade specified.
| Available Properties |
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Dart Drop Test
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|