Overview - Polypropylene, Blow Molding Grade
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: PP; Plastics, Polymers
| Available Properties |
- Density
- Water Absorption
- Moisture Vapor Transmission
- Oxygen Transmission
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched Low Temp
- Gardner Impact
- Low Temperature Gardner Impact
- Dart Drop Test
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|