Overview - Polypropylene, Film Grade
Subcategory: Polypropylene; Thermoplastic; Polymer
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: PP; Plastics, Polymers
| Available Properties |
- Density
- Moisture Vapor Transmission
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Secant Modulus
- Izod Impact, Notched
- Izod Impact, Unnotched
- Dart Drop Test
- Seal Strength
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Haze
- Gloss
- Transmission, Visible
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|