Overview - Thermoplastic Elastomer, Melt-Processible Rubber
Subcategory: Elastomer, TPE; Thermoplastic
Close Analogs: Click button for specific proprietary grades that belong to this Overview class.
Please be aware that some proprietary polymers may not be listed because they fall into more than one class or because of ambiguity in manufacturer's information.
Key Words: TPE; Plastics, Polymers
| Available Properties |
- Density
- Apparent Bulk Density
- Moisture Vapor Transmission
- Oxygen Transmission
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Shore A
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Poissons Ratio
- Gardner Impact
- Coefficient of Friction
- Compression Set
- Compression Set, Elevated Temperature
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- High Voltage Arc-Tracking Rate, HVTR
- CTE, linear 20°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Glass Temperature
- UL RTI, Electrical
- UL RTI, Mechanical without Impact
- Clash Berg Stiffness Temperature
- Flammability, UL94
- Oxygen Index
- Gloss
- Processing Temperature
- Rear Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|