Polynorbornene Rubber (PNR)
Subcategory: Elastomer, TS; Thermoset
Material Notes: High glass temperature - plasticizer needed to make a 'rubbery' compound.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Glass Temperature
|
|
|
|