Chlorosulfonated Polyethylene Rubber (CM, CSM)
Subcategory: Elastomer, TS; Thermoset
Key Words: CSM Trade Name: Hypalon
Material Notes: The chlorine (in CM) or chlorine and chlorosulfonyl (CSM) groups prevent the crystallization that occurs on unmodified polyethylene.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- CTE, linear 68°F
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
|
|
|
|
| Property Data |