Ethylene Propylene Rubber (EPM, EPDM)
Subcategory: Elastomer, TS; Thermoset
Key Words: ASTM D1418 EPM, EPDM; ASTM D2000 Designation CA, DA
Material Notes: Satisfactory compatibility with fireproof hydraulic fluids, ketones, hot and cold water, and alkalis. Unsatisfactory compatibility with most oils, gasoline, kerosene, aromatic and aliphatic hydrocarbons, halogenated solvents, and concentrated acids. Information provided by DuPont Dow Elastomers.
| Available Properties |
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- CTE, linear 68°F
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Glass Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|