Quadrant EPP Ertalyte® TX, Polyester-semi-crystalline thermoplastic with solid lubricant, extruded
Subcategory: Polyester, TP; Polyethylene Terephthalate (PET); Thermoplastic; Polymer; ; ; ; ; ; ;
Material Notes: Ertalyte TX is an extruded form of polyethylene terephthalate (PET-P) with a uniformly dispersed solid lubricant, providing superior wear resistance to most lubricated acetals and polyesters. In addition to having excellent wear properties, this material has excellent dimensional stability and remains stiff at elevated temperatures. Ertalyte TX is FDA compliant. Data provided by Quadrant Engineering Plastic Products.
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell M
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Strength
- Compressive Modulus
- Machinability (1-10; 1 = easiest)
- Dimensional Stability (1-4; 4 = highest)
- Shear Strength
- Coefficient of Friction
- K (wear) Factor
- Limiting Pressure Velocity
- Izod Impact, Notched
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Natural (off white)
- Grey
- FDA
- USDA
- 3A-Dairy
- Canada AG
- Acetaldehyde Aq. (40%)
- Acetic Acid Aq. (10%)
- Acetone
- Acrylonitrile
- Alcohols, Aliphatic
- Allyl Alcohol
- Aluminum Chloride Aq. (10%)
- Ammonia Aq. (10%)
- Ammonia Gas
- Ammonium Carbonate Aq. (10%)
- Ammonium Chloride Aq. (10%)
- Ammonium Chloride Aq. (37%)
- Amyl Acetate
- Amyl Alcohol
- Aniline
- Antimony Trichloride Aq. (10%)
- Barium Chloride Aq. (10%)
- Barium Sulfate Aq. (10%)
- Barium Sulfide Aq. (10%)
- Benzaldehyde
- Benzene
- Benzenesulfonic Acid
- Benzoic Acid Aq. (SAT)
- Benzyl Alcohol
- Beverages Aq. Alcoholic
- Beverages Aq. Carbonated
- Boric Acid Aq. (10%)
- Butanol
- Butyl Acetate
- Butyl Phthalate
- Butylene Glycol
- Butyric Acid Aq. (20%)
- Butyrolactone
- Calcium Chloride Aq. (10%)
- Calcium Hypochlorite
- Carbon Disulphide
- Carbon Tetrachloride
- Carbonic Acid Aq. (10%)
- Castor Oil
- Chlorine Gas (100%)
- Chloroacetic Acid Aq. (10%)
- Chlorobenzene
- Chloroform
- Chlorosulfonic Acid Aq. (10%)
- Chromic Acid Aq. (1%)
- Citric Acid Aq. (10%)
- Citric Acid Aq. (SAT)
- Cresylic Acid
- Cupric Chloride Aq. (10%)
- Cupric Sulfate Aq. (0.5%)
- Cupric Sulfate Aq. (10%)
- Cupric Sulfate Aq. (SAT)
- Cyclohexane
- Cyclohexanol
- Cyclohexanone
- Detergents, Organic
- Dibutylphthalate
- Dichlorodifluoro Methane
- Dichloroethylene
- Diesel Oil
- Diethyleneglycol Aq. (90%)
- Dimethyl Aniline
- Dimethyl Formamide
- Dioxane
- Edible Oils
- Ethanol, Denatured (96%)
- Ether, Diethyl
- Ethyl Acetate
- Ethyl Chloride
- Ethylene Chloride
- Ethylene Dichloride
- Ethylene Glycol Aq. (96%)
- Ferric Chloride Aq. (10%)
- Ferric Chloride Aq. (5%)
- Ferric Chloride Aq. (SAT)
- Ferrous Chloride Aq. (10%)
- Fluorine (Gas Wet)
- Fluorosilicic Acid Aq.
- Formaldehyde Aq. (10%)
- Formic Acid Aq. (10%)
- Formic Acid Aq. (3%)
- Freon 12 (Arcton 12)
- Fruit Juices (CONC)
- Furfural
- Gasoline
- Glycerine
- Heptane
- Hexane
- Hydrobromic Acid Aq. (10%)
- Hydrochloric Acid Aq. (0.4%)
- Hydrochloric Acid Aq. (10%)
- Hydrochloric Acid Aq. (2%)
- Hydrofluoric Acid Aq. (4%)
- Hydrogen Peroxide Aq. (0.5%)
- Hydrogen Peroxide Aq. (1%)
- Hydrogen Peroxide Aq. (3%)
- Hydrogen Sulfide Aq. (SAT)
- Hydrogenated Vegetable Oils
- Iodine (3%)
- Iodine (in Alcohol)
- Iso octane
- Isopropyl alcohol
- Isopropyl Ether
- Lactic Acid Aq. (10%)
- Lactic Acid Aq. (90%)
- Lead Acetate Aq. (10%)
- Lubricating Oils (Petroleum)
- Magnesium Chloride Aq. (10%)
- Magnesium Hydroxide Aq. (10%)
- Magnesium Sulfide Aq. (10%)
- Maleic Acid Aq. (CONC)
- Manganese Sulfate Aq. (10%)
- Mercury
- Methanol
- Methy Phenyl Ether
- Methyl Acetate
- Methyl Ethyl Ketone
- Methylene Chloride
- Milk
- Mineral Oils
- Naphthalene
- Nickel Sulfate Aq. (10%)
- Nitric Acid Aq. (0.1%)
- Nitric Acid Aq. (10%)
- Nitrobenzene
- Nitromethane
- Oleic Acid
- Oxalic Acid Aq. (10%)
- Ozone
- Paraffin
- Perchloric Acid Aq. (10%)
- Perchloroethylene
- Petroleum Ether
- Phenol (Molten)
- Phenol Aq. (6%)
- Phenol Aq. (75%)
- Phosphoric Acid Aq (0.3%)
- Phosphoric Acid Aq (3%)
- Phosphoric Acid Aq. (10%)
- Potassium Bicarbonate Aq. (60%)
- Potassium Bromide Aq. (10%)
- Potassium Carbonate Aq. (60%)
- Potassium Chloride Aq. (90%)
- Potassium Dichromate Aq. (5%)
- Potassium Hydroxide Aq. (10%)
- Potassium Hydroxide Aq. (50%)
- Potassium Nitrate Aq. (10%)
- Potassium Permanganate Aq. (1%)
- Propane Gas
- Pyridine
- Resorcinol
- Salicylic Acid
- Silicone Fluids
- Silver Nitrate
- Soap Solutions
- Sodium Acetate Aq. (60%)
- Sodium Benzoate Aq. (10%)
- Sodium Bicarbonate Aq. (50%)
- Sodium Bisulphite Aq. (10%)
- Sodium Bromide Aq. (10%)
- Sodium Carbonate Aq. (20%)
- Sodium Carbonate Aq. (50%)
- Sodium Chlorate Aq. (10%)
- Sodium Chloride Aq. (10%)
- Sodium Chloride Aq. (90%)
- Sodium Hydroxide Aq. (10%)
- Sodium Hydroxide Aq. (50%)
- Sodium Hypochlorite 15% CI (Chlorine Bleach)
- Sodium Nitrate Aq. (50%)
- Sodium Phosphates Aq. (General)
- Sodium Silicate
- Sodium Sulfate Aq. (90%)
- Sodium Sulfide Aq. (90%)
- Sodium Thiosulfate Aq. (10%)
- Stannic Chloride Aq. (10%)
- Styrene (Monomer)
- Sulfur
- Sulfur Dioxide (Dry Gas) (100%)
- Sulfuric Acid Aq. (2%)
- Sulfuric Acid Aq. (5%)
- Sulfuric Acid Conc.
- Tartaric Acid Aq.
- Tetrachlorethylene
- Tetrahydrofuran
- Tetralin
- Toluene
- Transformer Oil
- Trichlorethylene
- Triethanolamine
- Trisodium Phosphate Aq. (95%)
- Turpentine
- Urea
- Vaseline
- Vegetable Oils
- Vinegar
- Vinyl Chloride
- Water
- Wax (Molten)
- White Spirit
- Wines & Spirits
- Xylene
- Zinc Chloride Aq. (10%)
- Zinc Sulfate Aq. (10%)
- Compliance - FDA
- Machinability
- Service in Alcohols
- Service in Aliphatic Hydrocarbons
- Service in Aromatic Hydrocarbons
- Service in Chlorinated Solvents
- Service in Ethers
- Service in Ketones
- Service in Strong Acids
- Service in Strong Alkalies
- Service in Sunlight
- Service in Weak Acids
- Service in Weak Alkalies
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|