Quadrant EPP Ketron® PEEK LSG
Subcategory: Polyketone; Polyetheretherketone (PEEK); Thermoplastic
Material Notes: KETRON® PEEK LSG natural / black stock shapes are produced frombatches of Victrex PEEK. This material exhibits a unique combination of mechanical properties, temperature and chemical resistance. The composition of the resin used for the production of the KETRON® PEEK LSG stock shapes complies with the regulations that apply in the Member States of the European Union (Directive 2002/72/EC, as amended) and in the United States of America (FDA) for plastic materials and articles intended to come into contact with foodstuffs. KETRON PEEK LSG stock shapes have also been successfully type tested for their compliance with both United States Pharmacopeia (USP) and ISO 10993-1 guideline requirements for Biocompatibility Testing of Materials, and they come with full traceability from resin to stock shape. These features, added to an excellent sterilizability by means of steam, dry heat, ethylene oxide, plasma and gamma irradiation, make KETRON PEEK LSG stock shapes very suitable for applications in the medical, pharmaceutical and biotechnology markets.
| Available Properties |
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Yield Strength
- Compressive Strength
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|