Quadrant EPP Nylatron® MC® 901, Type 6, blue, heat stabilized, cast
Subcategory: Thermoplastic; Nylon 6; Polymer;
Material Notes: Data provided by Quadrant Engineering Plastic Products
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell M
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Strength
- Compressive Modulus
- Machinability (1-10; 1 = easiest)
- Dimensional Stability (1-4; 4 = highest)
- Shear Strength
- Coefficient of Friction
- K (wear) Factor
- Limiting Pressure Velocity
- Izod Impact, Notched
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- CTE, linear 68°F
- Thermal Conductivity
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Blue
- Acetaldehyde Aq. (40%)
- Acetamide Aq. (50%)
- Acetic Acid Aq. (10%)
- Acetone
- Acrylonitrile
- Alcohols, Aliphatic
- Allyl Alcohol
- Aluminum Chloride Aq. (10%)
- Aluminum Sulfate Aq. (10%)
- Ammonia Aq. (10%)
- Ammonia Gas
- Ammonium Carbonate Aq. (10%)
- Ammonium Chloride Aq. (10%)
- Ammonium Chloride Aq. (37%)
- Amyl Acetate
- Amyl Alcohol
- Aniline
- Antimony Trichloride Aq. (10%)
- Barium Chloride Aq. (10%)
- Barium Sulfate Aq. (10%)
- Benzaldehyde
- Benzene
- Benzoic Acid Aq. (SAT)
- Benzyl Alcohol
- Beverages Aq. Alcoholic
- Beverages Aq. Carbonated
- Bitumen
- Bleaching Lye (10%)
- Bleaching Lye (100%)
- Boric Acid Aq. (10%)
- Boron Trifluoride
- Bromine Aq. (30%)
- Bromine Liq.
- Butanol
- Butyl Acetate
- Butylene Glycol
- Butyric Acid (CONC)
- Butyric Acid Aq. (20%)
- Butyrolactone
- Calcium Chloride (in Alcohol) (20%)
- Calcium Chloride Aq. (10%)
- Calcium Hypochlorite
- Camphor
- Carbon Disulphide
- Carbon Tetrachloride
- Carnalite Aq. (10%)
- Catechol
- Chloral Hydrate
- Chlorine Aq. (10%)
- Chlorine Gas (100%)
- Chloroacetic Acid Aq. (10%)
- Chlorobenzene
- Chloroform
- Chlorosulfonic Acid Aq. (10%)
- Chromic Acid Aq. (1%)
- Citric Acid Aq. (10%)
- Citric Acid Aq. (SAT)
- Coconut Oil
- Cresols
- Cupric Sulfate Aq. (0.5%)
- Cupric Sulfate Aq. (SAT)
- Cyclohexane
- Cyclohexanol
- Cyclohexanone
- Decalin
- Detergents, Organic
- Dibutylphthalate
- Dichlorodifluoro Methane
- Dichloroethylene
- Diesel Oil
- Diethyleneglycol Aq. (90%)
- Dimethyl Carbinol
- Dimethyl Formamide
- Dioxane
- Edible Oils
- Ethanol, Denatured (96%)
- Ether, Diethyl
- Ethyl Acetate
- Ethyl Chloride
- Ethylene Chloride
- Ethylene Diamine
- Ethylene Glycol Aq. (96%)
- Ferric Chloride Aq. (5%)
- Ferric Chloride Aq. (SAT)
- Ferrous Chloride Aq. (10%)
- Fluorine (Gas Wet)
- Fluorosilicic Acid Aq.
- Fluothane
- Formaldehyde Aq. (10%)
- Formic Acid Aq. (10%)
- Formic Acid Aq. (3%)
- Freon 12 (Arcton 12)
- Fruit Juices (CONC)
- Furfural
- Gasoline
- Glycerine
- Heptane
- Hexane
- Hydrobromic Acid Aq. (10%)
- Hydrochloric Acid Aq. (0.4%)
- Hydrochloric Acid Aq. (10%)
- Hydrochloric Acid Aq. (2%)
- Hydrofluoric Acid Aq. (4%)
- Hydrogen Peroxide Aq. (1%)
- Hydrogen Peroxide Aq. (3%)
- Hydrogen Sulfide Aq. (SAT)
- Hydrogenated Vegetable Oils
- Hydroquinone
- Iodine (3%)
- Iodine (in Alcohol)
- Iso octane
- Isopropyl alcohol
- Isopropyl Ether
- Lactic Acid Aq. (10%)
- Lactic Acid Aq. (90%)
- Lead Acetate Aq. (10%)
- Lead Stearate
- Linseed Oil
- Lithium Bromide Aq. (50%)
- Lubricating Oils (Petroleum)
- Magnesium Chloride Aq. (10%)
- Magnesium Hydroxide Aq. (10%)
- Magnesium Sulfide Aq. (10%)
- Maleic Acid Aq. (CONC)
- Malonic Acid Aq. (CONC)
- Manganese Sulfate Aq. (10%)
- Mercuric Chloride Aq. (6%)
- Mercury
- Methanol
- Methyl Acetate
- Methyl Ethyl Ketone
- Methylene Chloride
- Methylpyrrolidone
- Milk
- Mineral Oils
- Naphthalene
- Nickel Sulfate Aq. (10%)
- Nicotine
- Nitric Acid Aq. (0.1%)
- Nitric Acid Aq. (10%)
- Nitrobenzene
- Nitromethane
- Oleic Acid
- Oxalic Acid Aq. (10%)
- Ozone
- Paraffin
- Perchloric Acid Aq. (10%)
- Perchloroethylene
- Petroleum Ether
- Phenol (Molten)
- Phenol Aq. (6%)
- Phenol Aq. (75%)
- Phosphoric Acid Aq (0.3%)
- Phosphoric Acid Aq (3%)
- Phosphoric Acid Aq. (10%)
- Phthalic Acid Aq. (SAT)
- Phthalic Dioctyl
- Potassium Acetate Aq. (50%)
- Potassium Bicarbonate Aq. (60%)
- Potassium Bromide Aq. (10%)
- Potassium Carbonate Aq. (60%)
- Potassium Chloride Aq. (90%)
- Potassium Dichromate Aq. (5%)
- Potassium Ferricyanide Aq. (30%)
- Potassium Ferrocyanide Aq. (30%)
- Potassium Hydroxide Aq. (10%)
- Potassium Hydroxide Aq. (50%)
- Potassium Nitrate Aq. (10%)
- Potassium Permanganate Aq. (1%)
- Potassium Sulfite Aq. (CONC)
- Propane Gas
- Pyridine
- Resorcinol
- Salicylic Acid
- Silicone Fluids
- Silver Nitrate
- Soap Solutions
- Sodium Acetate Aq. (60%)
- Sodium Bicarbonate Aq. (50%)
- Sodium Bisulphite Aq. (10%)
- Sodium Bromide Aq. (10%)
- Sodium Carbonate Aq. (20%)
- Sodium Chlorate Aq. (10%)
- Sodium Chloride Aq. (10%)
- Sodium Chloride Aq. (90%)
- Sodium Hydroxide Aq. (10%)
- Sodium Hydroxide Aq. (50%)
- Sodium Hypochlorite 15% CI (Chlorine Bleach)
- Sodium Nitrate Aq. (50%)
- Sodium Silicate
- Sodium Sulfate Aq. (90%)
- Sodium Thiosulfate Aq. (10%)
- Stannic Sulfate Aq. (10%)
- Stearic Acid
- Styrene (Monomer)
- Sulfur
- Sulfur Dioxide (Dry Gas) (100%)
- Sulfuric Acid Aq. (2%)
- Sulfuric Acid Aq. (5%)
- Sulfuric Acid Conc.
- Tallow
- Tar
- Tartaric Acid Aq.
- Tetrachlorethylene
- Tetrahydrofuran
- Tetralin
- Thionyl Chloride
- Toluene
- Transformer Oil
- Trichlorethylene
- Triethanolamine
- Trisodium Phosphate Aq. (95%)
- Turpentine
- Urea
- Vaseline
- Vegetable Oils
- Vinegar
- Vinyl Chloride
- Water
- Wax (Molten)
- White Spirit
- Wines & Spirits
- Xylene
- Xylenol
- Zinc Chloride Aq. (10%)
- Zinc Oxide
- Compliance - FDA
- Machinability
- Service in Alcohols
- Service in Aliphatic Hydrocarbons
- Service in Aromatic Hydrocarbons
- Service in Chlorinated Solvents
- Service in Ethers
- Service in Ketones
- Service in Strong Acids
- Service in Strong Alkalies
- Service in Sunlight
- Service in Weak Acids
- Service in Weak Alkalies
|
|
|
|
| Property Data |
This page displays only the text