Quadrant EPP Semitron® ESd 410C (CM), Polyetherimide, static dissipative, compression molded
Subcategory: Polyetherimide; Thermoplastic; Polymer
Material Notes: Semitron ESd 410C is part of the Quadrant EPP family of products designed for use in the semiconductor industry, where electrostatic dissipation is a requirement. It is a compression-molded, static dissipative polyetherimide that performs at temperatures up to 410°F and has surface resistivity in the conductive range. Data provided by Quadrant Engineering Plastic Products.
| Available Properties |
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell M
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Strength
- Compressive Modulus
- Dimensional Stability (1-4; 4 = highest)
- Shear Strength
- Coefficient of Friction
- K (wear) Factor
- Limiting Pressure Velocity
- Izod Impact, Notched
- Surface Resistivity per Square
- Dielectric Constant
- Dissipation Factor
- CTE, linear 68°F
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Black
- Compliance - FDA
- Machinability
- Service in Alcohols
- Service in Aliphatic Hydrocarbons
- Service in Aromatic Hydrocarbons
- Service in Chlorinated Solvents
- Service in Ethers
- Service in Ketones
- Service in Strong Acids
- Service in Strong Alkalies
- Service in Sunlight
- Service in Weak Acids
- Service in Weak Alkalies
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|