Quadrant EPP Semitron® ESd 420 Polyetherimide, static dissipative, compression molded
Subcategory: Polyetherimide; Polysulfone; Thermoplastic; Polymer; ; ; ; ; ; ;
Key Words: PEI
Material Notes: Semitron ESd 420 is part of the Quadrant EPP family of products designed for use in the semiconductor industry, where electrostatic dissipation is a requirement. It is a compression-molded material that performs at temperatures to 410 and is designed for applications currently in PEI or PES, but where protection from static discharge is required. Data provided by Quadrant Engineering Plastic Products.
| Available Properties |
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Strength
- Compressive Modulus
- Machinability (1-10; 1 = easiest)
- Dimensional Stability (1-4; 4 = highest)
- Shear Strength
- Coefficient of Friction
- K (wear) Factor
- Limiting Pressure Velocity
- Izod Impact, Notched
- Surface Resistivity per Square
- Dielectric Constant
- Dissipation Factor
- CTE, linear 68°F
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Black
- FDA
- USDA
- NSF
- USP Class VI available
- Autoclavable
- Acetaldehyde Aq. (40%)
- Acetic Acid Aq. (10%)
- Acetone
- Alcohols, Aliphatic
- Ammonia Aq. (10%)
- Amyl Acetate
- Benzaldehyde
- Benzene
- Benzoic Acid Aq. (SAT)
- Beverages Aq. Alcoholic
- Beverages Aq. Carbonated
- Butanol
- Butyl Acetate
- Butylamine
- Butylene Glycol
- Carbon Tetrachloride
- Chloroform
- Chromic Acid Aq. (1%)
- Citric Acid Aq. (10%)
- Citric Acid Aq. (SAT)
- Cyclohexane
- Cyclohexanol
- Decalin
- Detergents, Organic
- Dibutylphthalate
- Dichlorodifluoro Methane
- Dichloroethylene
- Diesel Oil
- Dimethyl Formamide
- Edible Oils
- Ethanol, Denatured (96%)
- Ether, Diethyl
- Ethyl Acetate
- Ethyl Butyrate
- Ethylene Chloride
- Ethylene Diamine
- Ethylene Dichloride
- Ethylene Glycol Aq. (96%)
- Ferrous Chloride Aq. (10%)
- Formaldehyde Aq. (10%)
- Formic Acid Aq. (10%)
- Formic Acid Aq. (3%)
- Freon 12 (Arcton 12)
- Gasoline
- Glycerine
- Heptane
- Hexane
- Hydrochloric Acid Aq. (0.4%)
- Hydrochloric Acid Aq. (10%)
- Hydrochloric Acid Aq. (2%)
- Hydrofluoric Acid Aq. (4%)
- Hydrogen Peroxide Aq. (0.5%)
- Hydrogen Peroxide Aq. (1%)
- Hydrogen Peroxide Aq. (3%)
- Hydrogen Sulfide Aq. (SAT)
- Iodine (3%)
- Iso octane
- Isopropyl alcohol
- Isopropyl Ether
- Lubricating Oils (Petroleum)
- Methanol
- Methyl Acetate
- Methyl Ethyl Ketone
- Methylene Chloride
- Milk
- Mineral Oils
- Naphthalene
- Nitric Acid Aq. (0.1%)
- Nitric Acid Aq. (10%)
- Nitrobenzene
- Oxalic Acid Aq. (10%)
- Ozone
- Paraffin
- Perchloroethylene
- Petroleum Ether
- Phenol (Molten)
- Phenol Aq. (6%)
- Phenol Aq. (75%)
- Phosphoric Acid Aq (0.3%)
- Phosphoric Acid Aq (3%)
- Phosphoric Acid Aq. (10%)
- Potassium Carbonate Aq. (60%)
- Potassium Hydroxide Aq. (10%)
- Potassium Hydroxide Aq. (50%)
- Propane Gas
- Silicone Fluids
- Soap Solutions
- Sodium Acetate Aq. (60%)
- Sodium Benzoate Aq. (10%)
- Sodium Bicarbonate Aq. (50%)
- Sodium Bisulphite Aq. (10%)
- Sodium Carbonate Aq. (20%)
- Sodium Carbonate Aq. (50%)
- Sodium Chlorate Aq. (10%)
- Sodium Chloride Aq. (10%)
- Sodium Chloride Aq. (90%)
- Sodium Cyanide Aq. (10%)
- Sodium Hydroxide Aq. (10%)
- Sodium Hydroxide Aq. (50%)
- Sodium Hypochlorite 15% CI (Chlorine Bleach)
- Sodium Nitrate Aq. (50%)
- Sodium Perborate Aq. (10%)
- Sodium Phosphates Aq. (General)
- Sodium Silicate
- Sodium Sulfate Aq. (90%)
- Sodium Sulfide Aq. (90%)
- Sodium Thiosulfate Aq. (10%)
- Stannic Chloride Aq. (10%)
- Sulfuric Acid Aq. (2%)
- Sulfuric Acid Aq. (5%)
- Sulfuric Acid Conc.
- Sulfurous Acid Aq. (10%)
- Tallow
- Tetrachlorethylene
- Tetrahydrofuran
- Toluene
- Trichlorethylene
- Triethanolamine
- Trisodium Phosphate Aq. (95%)
- Vaseline
- Vegetable Oils
- Vinegar
- Vinyl Chloride
- Water
- Wax (Molten)
- Wines & Spirits
- Xylene
- Xylenol
- Zinc Chloride Aq. (10%)
- Compliance - FDA
- Machinability
- Service in Alcohols
- Service in Aliphatic Hydrocarbons
- Service in Aromatic Hydrocarbons
- Service in Chlorinated Solvents
- Service in Ethers
- Service in Ketones
- Service in Strong Acids
- Service in Strong Alkalies
- Service in Sunlight
- Service in Weak Acids
- Service in Weak Alkalies
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|