Quadrant EPP Semitron® ESd 520HR (CM), Polyamide-imide, static dissipative, compression molded

 

Subcategory: Polyamide-imide; Thermoplastic; Polymer;

Key Words: PAI

Material Notes:
Semitron ESd 520HR is part of the Quadrant EPP family of products designed for use in the semiconductor industry, where electrostatic dissipation is a requirement. It is a compression-molded, static dissipative PAI that combines high heat and chemical resistance with incredible dimensional stability. It also offers consistent static dissipation that withstands exposure to higher voltages without dielectric breakdown.

Data provided by Quadrant Engineering Plastic Products.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Water Absorption at Saturation
  • Hardness, Rockwell M
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Yield Strength
  • Compressive Strength
  • Compressive Modulus
  • Machinability (1-10; 1 = easiest)
  • Dimensional Stability (1-4; 4 = highest)
  • Shear Strength
  • Coefficient of Friction
  • K (wear) Factor
  • Limiting Pressure Velocity
  • Izod Impact, Notched
  • Surface Resistivity per Square
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 68°F
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Glass Temperature
  • Flammability, UL94
  • Black
  • Acetaldehyde Aq. (40%)
  • Acetic Acid Aq. (10%)
  • Acetone
  • Acrylonitrile
  • Alcohols, Aliphatic
  • Allyl Alcohol
  • Aluminum Chloride Aq. (10%)
  • Aluminum Sulfate Aq. (10%)
  • Ammonia Aq. (10%)
  • Ammonia Gas
  • Ammonium Carbonate Aq. (10%)
  • Ammonium Chloride Aq. (10%)
  • Ammonium Chloride Aq. (37%)
  • Amyl Acetate
  • Amyl Alcohol
  • Aniline
  • Barium Chloride Aq. (10%)
  • Barium Sulfate Aq. (10%)
  • Barium Sulfide Aq. (10%)
  • Benzaldehyde
  • Benzene
  • Benzenesulfonic Acid
  • Benzyl Alcohol
  • Beverages Aq. Alcoholic
  • Beverages Aq. Carbonated
  • Bleaching Lye (10%)
  • Bromine Aq. (30%)
  • Bromine Liq.
  • Butanol
  • Butyl Acetate
  • Butyl Phthalate
  • Butylamine
  • Butyrolactone
  • Calcium Chloride Aq. (10%)
  • Calcium Hypochlorite
  • Carbon Tetrachloride
  • Chlorobenzene
  • Chloroform
  • Chromic Acid Aq. (1%)
  • Cyclohexane
  • Cyclohexanol
  • Cyclohexanone
  • Dibutylphthalate
  • Dichloroethylene
  • Diesel Oil
  • Diethyleneglycol Aq. (90%)
  • Dimethyl Aniline
  • Dioxane
  • Edible Oils
  • Ethanol, Denatured (96%)
  • Ether, Diethyl
  • Ethyl Acetate
  • Ethyl Butyrate
  • Ethyl Chloride
  • Ethylene Chloride
  • Ethylene Chlorohydrin
  • Ethylene Diamine
  • Ethylene Dichloride
  • Ethylene Glycol Aq. (96%)
  • Ethylene Propionate
  • Ferric Chloride Aq. (10%)
  • Ferric Chloride Aq. (5%)
  • Ferric Chloride Aq. (SAT)
  • Ferrous Chloride Aq. (10%)
  • Formaldehyde Aq. (10%)
  • Formic Acid Aq. (10%)
  • Formic Acid Aq. (3%)
  • Fruit Juices (CONC)
  • Furfural
  • Gasoline
  • Glycerine
  • Heptane
  • Hexane
  • Hydrobromic Acid Aq. (10%)
  • Hydrochloric Acid Aq. (0.4%)
  • Hydrochloric Acid Aq. (10%)
  • Hydrochloric Acid Aq. (2%)
  • Hydrofluoric Acid Aq. (4%)
  • Hydrogen Sulfide Aq. (SAT)
  • Hydrogenated Vegetable Oils
  • Iso octane
  • Isopropyl alcohol
  • Isopropyl Ether
  • Lactic Acid Aq. (10%)
  • Lactic Acid Aq. (90%)
  • Lead Acetate Aq. (10%)
  • Lubricating Oils (Petroleum)
  • Magnesium Chloride Aq. (10%)
  • Magnesium Hydroxide Aq. (10%)
  • Magnesium Sulfide Aq. (10%)
  • Methanol
  • Methy Phenyl Ether
  • Methyl Acetate
  • Methyl Ethyl Ketone
  • Methylene Chloride
  • Milk
  • Mineral Oils
  • Nickel Sulfate Aq. (10%)
  • Nitric Acid Aq. (0.1%)
  • Nitric Acid Aq. (10%)
  • Nitrobenzene
  • Nitromethane
  • Paraffin
  • Perchloric Acid Aq. (10%)
  • Perchloroethylene
  • Petroleum Ether
  • Phosphoric Acid Aq (0.3%)
  • Phosphoric Acid Aq (3%)
  • Phosphoric Acid Aq. (10%)
  • Potassium Acetate Aq. (50%)
  • Potassium Bicarbonate Aq. (60%)
  • Potassium Bromide Aq. (10%)
  • Potassium Carbonate Aq. (60%)
  • Potassium Chloride Aq. (90%)
  • Potassium Dichromate Aq. (5%)
  • Potassium Hydroxide Aq. (10%)
  • Potassium Hydroxide Aq. (50%)
  • Potassium Permanganate Aq. (1%)
  • Potassium Sulfite Aq. (CONC)
  • Pyridine
  • Silicone Fluids
  • Silver Nitrate
  • Soap Solutions
  • Sodium Acetate Aq. (60%)
  • Sodium Benzoate Aq. (10%)
  • Sodium Bicarbonate Aq. (50%)
  • Sodium Bisulphite Aq. (10%)
  • Sodium Bromide Aq. (10%)
  • Sodium Carbonate Aq. (20%)
  • Sodium Carbonate Aq. (50%)
  • Sodium Chlorate Aq. (10%)
  • Sodium Chloride Aq. (10%)
  • Sodium Chloride Aq. (90%)
  • Sodium Cyanide Aq. (10%)
  • Sodium Hydroxide Aq. (10%)
  • Sodium Hydroxide Aq. (50%)
  • Sodium Hypochlorite 15% CI (Chlorine Bleach)
  • Sodium Perborate Aq. (10%)
  • Sodium Phosphates Aq. (General)
  • Sodium Silicate
  • Sodium Sulfate Aq. (90%)
  • Sodium Sulfide Aq. (90%)
  • Sodium Thiosulfate Aq. (10%)
  • Sulfur Dioxide (Dry Gas) (100%)
  • Sulfuric Acid Aq. (2%)
  • Sulfuric Acid Aq. (5%)
  • Sulfuric Acid Conc.
  • Tallow
  • Tar
  • Tetrachlorethylene
  • Tetrahydrofuran
  • Toluene
  • Transformer Oil
  • Trichlorethylene
  • Triethanolamine
  • Trisodium Phosphate Aq. (95%)
  • Turpentine
  • Vaseline
  • Vegetable Oils
  • Vinegar
  • Vinyl Chloride
  • Water
  • Wax (Molten)
  • White Spirit
  • Wines & Spirits
  • Xylene
  • Xylenol
  • Compliance - FDA
  • Machinability
  • Service in Alcohols
  • Service in Aliphatic Hydrocarbons
  • Service in Aromatic Hydrocarbons
  • Service in Chlorinated Solvents
  • Service in Ethers
  • Service in Ketones
  • Service in Strong Acids
  • Service in Strong Alkalies
  • Service in Sunlight
  • Service in Weak Acids
  • Service in Weak Alkalies
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。