Quadrant EPP Duratron® T4540 PAI, Polyamide-imide, compression molded (bearing grade)
Subcategory: Polyamide-imide; Thermoplastic; Polymer;
Key Words: Quadrant Engineering Plastics Products
Material Notes: Duratron® T4540 compression molded PAI is a seal and bearing grade offers a very low coefficient of friction and good wear properties. It was developed specifically for use in rotating equipment. Its composition is the same as the former Duratron® T4340 polyamide-imide and used when larger (especially tubular) shapes are required. Typical applications for Duratron® T4540 PAI include labyrinth seals, wear rings, bushings, and bearings of all types. Duratron® PAI is the highest performing melt processable plastic. It has superior resistance to elevated temperatures. It is capable of performing under severe stress conditions at continuous temperatures to 500°F (260°C). Parts machined from Duratron® PAI stock shapes provide greater compressive strength and higher impact resistance than most advanced engineering plastics. Its extremely low coefficient of linear thermal expansion and high creep resistance deliver excellent dimensional stability over its entire use range. Duratron® PAI is an amorphous material with a Tg (glass transition temperature) of 537°F (280°C). Data provided by Quadrant Engineering Plastic Products from tests on stock shapes and parts produced by Quadrant EPP.
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell E
- Hardness, Rockwell M
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Strength
- Compressive Modulus
- Machinability (1-10; 1 = easiest)
- Dimensional Stability (1-4; 4 = highest)
- Coefficient of Friction
- K (wear) Factor
- Limiting Pressure Velocity
- Izod Impact, Notched
- Surface Resistivity per Square
- CTE, linear 68°F
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Black
- Outgassing (% TML) (1-4; 4 = highest)
- Acetaldehyde Aq. (40%)
- Acetic Acid Aq. (10%)
- Acetone
- Acrylonitrile
- Alcohols, Aliphatic
- Allyl Alcohol
- Aluminum Chloride Aq. (10%)
- Aluminum Sulfate Aq. (10%)
- Ammonia Aq. (10%)
- Ammonia Gas
- Ammonium Carbonate Aq. (10%)
- Ammonium Chloride Aq. (10%)
- Ammonium Chloride Aq. (37%)
- Amyl Acetate
- Amyl Alcohol
- Aniline
- Barium Chloride Aq. (10%)
- Barium Sulfate Aq. (10%)
- Barium Sulfide Aq. (10%)
- Benzaldehyde
- Benzene
- Benzenesulfonic Acid
- Benzyl Alcohol
- Beverages Aq. Alcoholic
- Beverages Aq. Carbonated
- Bleaching Lye (10%)
- Bromine Aq. (30%)
- Bromine Liq.
- Butanol
- Butyl Acetate
- Butyl Phthalate
- Butylamine
- Butyrolactone
- Calcium Chloride Aq. (10%)
- Calcium Hypochlorite
- Carbon Tetrachloride
- Chlorobenzene
- Chloroform
- Chromic Acid Aq. (1%)
- Cyclohexane
- Cyclohexanol
- Cyclohexanone
- Dibutylphthalate
- Dichloroethylene
- Diesel Oil
- Diethyleneglycol Aq. (90%)
- Dimethyl Aniline
- Dioxane
- Edible Oils
- Ethanol, Denatured (96%)
- Ether, Diethyl
- Ethyl Acetate
- Ethyl Butyrate
- Ethyl Chloride
- Ethylene Chloride
- Ethylene Chlorohydrin
- Ethylene Diamine
- Ethylene Dichloride
- Ethylene Glycol Aq. (96%)
- Ethylene Propionate
- Ferric Chloride Aq. (10%)
- Ferric Chloride Aq. (5%)
- Ferric Chloride Aq. (SAT)
- Ferrous Chloride Aq. (10%)
- Formaldehyde Aq. (10%)
- Formic Acid Aq. (10%)
- Formic Acid Aq. (3%)
- Fruit Juices (CONC)
- Furfural
- Gasoline
- Glycerine
- Heptane
- Hexane
- Hydrobromic Acid Aq. (10%)
- Hydrochloric Acid Aq. (0.4%)
- Hydrochloric Acid Aq. (10%)
- Hydrochloric Acid Aq. (2%)
- Hydrofluoric Acid Aq. (4%)
- Hydrogen Sulfide Aq. (SAT)
- Hydrogenated Vegetable Oils
- Iso octane
- Isopropyl alcohol
- Isopropyl Ether
- Lactic Acid Aq. (10%)
- Lactic Acid Aq. (90%)
- Lead Acetate Aq. (10%)
- Lubricating Oils (Petroleum)
- Magnesium Chloride Aq. (10%)
- Magnesium Hydroxide Aq. (10%)
- Magnesium Sulfide Aq. (10%)
- Methanol
- Methy Phenyl Ether
- Methyl Acetate
- Methyl Ethyl Ketone
- Methylene Chloride
- Milk
- Mineral Oils
- Nickel Sulfate Aq. (10%)
- Nitric Acid Aq. (0.1%)
- Nitric Acid Aq. (10%)
- Nitrobenzene
- Nitromethane
- Paraffin
- Perchloric Acid Aq. (10%)
- Perchloroethylene
- Petroleum Ether
- Phosphoric Acid Aq (0.3%)
- Phosphoric Acid Aq (3%)
- Phosphoric Acid Aq. (10%)
- Potassium Acetate Aq. (50%)
- Potassium Bicarbonate Aq. (60%)
- Potassium Bromide Aq. (10%)
- Potassium Carbonate Aq. (60%)
- Potassium Chloride Aq. (90%)
- Potassium Dichromate Aq. (5%)
- Potassium Hydroxide Aq. (10%)
- Potassium Hydroxide Aq. (50%)
- Potassium Permanganate Aq. (1%)
- Potassium Sulfite Aq. (CONC)
- Pyridine
- Silicone Fluids
- Silver Nitrate
- Soap Solutions
- Sodium Acetate Aq. (60%)
- Sodium Benzoate Aq. (10%)
- Sodium Bicarbonate Aq. (50%)
- Sodium Bisulphite Aq. (10%)
- Sodium Bromide Aq. (10%)
- Sodium Carbonate Aq. (20%)
- Sodium Carbonate Aq. (50%)
- Sodium Chlorate Aq. (10%)
- Sodium Chloride Aq. (10%)
- Sodium Chloride Aq. (90%)
- Sodium Cyanide Aq. (10%)
- Sodium Hydroxide Aq. (10%)
- Sodium Hydroxide Aq. (50%)
- Sodium Hypochlorite 15% CI (Chlorine Bleach)
- Sodium Perborate Aq. (10%)
- Sodium Phosphates Aq. (General)
- Sodium Silicate
- Sodium Sulfate Aq. (90%)
- Sodium Sulfide Aq. (90%)
- Sodium Thiosulfate Aq. (10%)
- Sulfur Dioxide (Dry Gas) (100%)
- Sulfuric Acid Aq. (2%)
- Sulfuric Acid Aq. (5%)
- Sulfuric Acid Conc.
- Tallow
- Tar
- Tetrachlorethylene
- Tetrahydrofuran
- Toluene
- Transformer Oil
- Trichlorethylene
- Triethanolamine
- Trisodium Phosphate Aq. (95%)
- Turpentine
- Vaseline
- Vegetable Oils
- Vinegar
- Vinyl Chloride
- Water
- Wax (Molten)
- White Spirit
- Wines & Spirits
- Xylene
- Xylenol
- Compliance - FDA
- Machinability
- Service in Alcohols
- Service in Aliphatic Hydrocarbons
- Service in Aromatic Hydrocarbons
- Service in Chlorinated Solvents
- Service in Ethers
- Service in Ketones
- Service in Strong Acids
- Service in Strong Alkalies
- Service in Sunlight
- Service in Weak Acids
- Service in Weak Alkalies
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|