Quadrant EPP Duratron® U1000 PEI, Polyetherimide, unfilled, extruded
Subcategory: Polyetherimide; Thermoplastic; Polymer; ; ; ; ; ; ;
Close Analogs: Formerly SABIC Innovative Plastics Ultem® 1000 PEI.
Key Words: Quadrant Engineering Plastics Products; PEI
Material Notes: Duratron® U1000 polyetherimide is an amorphous, high-performance polymer with exceptional flame and heat resistance. It performs continuously to 340°F (171°C), making it ideal for high strength/high heat applications, and those requiring consistent dielectric properties over a wide frequency range. It is hydrolysis resistant, highly resistant to acidic solutions and capable of withstanding multiple autoclaving cycles. Duratron® U1000 is FDA and USP Class VI compliant. FDA compliant colors of Duratron® PEI are also available on a custom basis. Duratron® PEI commonly is machined into parts for reusable medical devices, analytical instrumentation, electrical/electronic insulators and a variety of structural components requiring high strength and rigidity at elevated temperatures. Data provided by Quadrant Engineering Plastic Products from tests on stock shapes and parts produced by Quadrant EPP.
| Available Properties |
- Cost, 1 to 10 (Nylon = 2)
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Hardness, Rockwell M
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Strength
- Compressive Modulus
- Machinability (1-10; 1 = easiest)
- Dimensional Stability (1-4; 4 = highest)
- Shear Strength
- Coefficient of Friction
- K (wear) Factor
- Limiting Pressure Velocity
- Izod Impact, Notched
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- CTE, linear 68°F
- Thermal Conductivity
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Glass Temperature
- Flammability, UL94
- Black
- Amber
- Transparent
- FDA
- USDA
- NSF
- USP Class VI available
- Autoclavable
- UV Resistance (1-4; 4 = highest)
- Outgassing (% TML) (1-4; 4 = highest)
- Acetaldehyde Aq. (40%)
- Acetic Acid Aq. (10%)
- Acetone
- Alcohols, Aliphatic
- Ammonia Aq. (10%)
- Amyl Acetate
- Benzaldehyde
- Benzene
- Benzoic Acid Aq. (SAT)
- Beverages Aq. Alcoholic
- Beverages Aq. Carbonated
- Butanol
- Butyl Acetate
- Butylamine
- Butylene Glycol
- Carbon Tetrachloride
- Chloroform
- Chromic Acid Aq. (1%)
- Citric Acid Aq. (10%)
- Citric Acid Aq. (SAT)
- Cyclohexane
- Cyclohexanol
- Decalin
- Detergents, Organic
- Dibutylphthalate
- Dichlorodifluoro Methane
- Dichloroethylene
- Diesel Oil
- Dimethyl Formamide
- Edible Oils
- Ethanol, Denatured (96%)
- Ether, Diethyl
- Ethyl Acetate
- Ethyl Butyrate
- Ethylene Chloride
- Ethylene Diamine
- Ethylene Dichloride
- Ethylene Glycol Aq. (96%)
- Ferrous Chloride Aq. (10%)
- Formaldehyde Aq. (10%)
- Formic Acid Aq. (10%)
- Formic Acid Aq. (3%)
- Freon 12 (Arcton 12)
- Gasoline
- Glycerine
- Heptane
- Hexane
- Hydrochloric Acid Aq. (0.4%)
- Hydrochloric Acid Aq. (10%)
- Hydrochloric Acid Aq. (2%)
- Hydrofluoric Acid Aq. (4%)
- Hydrogen Peroxide Aq. (0.5%)
- Hydrogen Peroxide Aq. (1%)
- Hydrogen Peroxide Aq. (3%)
- Hydrogen Sulfide Aq. (SAT)
- Iodine (3%)
- Iso octane
- Isopropyl alcohol
- Isopropyl Ether
- Lubricating Oils (Petroleum)
- Methanol
- Methyl Acetate
- Methyl Ethyl Ketone
- Methylene Chloride
- Milk
- Mineral Oils
- Naphthalene
- Nitric Acid Aq. (0.1%)
- Nitric Acid Aq. (10%)
- Nitrobenzene
- Oxalic Acid Aq. (10%)
- Ozone
- Paraffin
- Perchloroethylene
- Petroleum Ether
- Phenol (Molten)
- Phenol Aq. (6%)
- Phenol Aq. (75%)
- Phosphoric Acid Aq (0.3%)
- Phosphoric Acid Aq (3%)
- Phosphoric Acid Aq. (10%)
- Potassium Carbonate Aq. (60%)
- Potassium Hydroxide Aq. (10%)
- Potassium Hydroxide Aq. (50%)
- Propane Gas
- Silicone Fluids
- Soap Solutions
- Sodium Acetate Aq. (60%)
- Sodium Benzoate Aq. (10%)
- Sodium Bicarbonate Aq. (50%)
- Sodium Bisulphite Aq. (10%)
- Sodium Carbonate Aq. (20%)
- Sodium Carbonate Aq. (50%)
- Sodium Chlorate Aq. (10%)
- Sodium Chloride Aq. (10%)
- Sodium Chloride Aq. (90%)
- Sodium Cyanide Aq. (10%)
- Sodium Hydroxide Aq. (10%)
- Sodium Hydroxide Aq. (50%)
- Sodium Hypochlorite 15% CI (Chlorine Bleach)
- Sodium Nitrate Aq. (50%)
- Sodium Perborate Aq. (10%)
- Sodium Phosphates Aq. (General)
- Sodium Silicate
- Sodium Sulfate Aq. (90%)
- Sodium Sulfide Aq. (90%)
- Sodium Thiosulfate Aq. (10%)
- Stannic Chloride Aq. (10%)
- Sulfuric Acid Aq. (2%)
- Sulfuric Acid Aq. (5%)
- Sulfuric Acid Conc.
- Sulfurous Acid Aq. (10%)
- Tallow
- Tetrachlorethylene
- Tetrahydrofuran
- Toluene
- Trichlorethylene
- Triethanolamine
- Trisodium Phosphate Aq. (95%)
- Vaseline
- Vegetable Oils
- Vinegar
- Vinyl Chloride
- Water
- Wax (Molten)
- Wines & Spirits
- Xylene
- Xylenol
- Zinc Chloride Aq. (10%)
- Compliance - FDA
- Machinability
- Service in Alcohols
- Service in Aliphatic Hydrocarbons
- Service in Aromatic Hydrocarbons
- Service in Chlorinated Solvents
- Service in Ethers
- Service in Ketones
- Service in Strong Acids
- Service in Strong Alkalies
- Service in Sunlight
- Service in Weak Acids
- Service in Weak Alkalies
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|