Chevron Phillips MarFlex™ PE 7120S LLDPE Blown & Cast Film Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Linear Low Density Polyethylene
Material Notes: Resin Type: linear low density polyethylene, hexene copolymer with enhanced stabilization package Characteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE, no process aid. Applications: stretch wrap, overwrap, coextrusions Recommended processing conditions: 6.35 cm extruder. 24:1 screw L/D ratio. 0.064 cm die opening. Melt temperature 270°C. Data provided by Chevron Phillips Chemical Company, LP.
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Coefficient of Friction
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Haze
- Gloss
- Processing Temperature
- Die Opening
- Extruder Size
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|