Chevron Phillips K-Resin® BK11 Styrene-Butadiene Copolymer, Injection Molding Grade

 

Subcategory: Styrene-Butadiene; Thermoplastic

Key Words: SBC Poly(Styrene Butadiene)

Material Notes:
Styrene-Butadiene Copolymer

Customer Benefits: BK11 is an SBC consisting of our commercial KR03 grade with a mold release added of easier processing. BK11 molded parts give excellent detail on fast production cycles, and are easily processed by injection molding. This resin can be tinted or colored in a variety of transparent and opaque shades. Compared to KR03, BK11 offers improved mold release with the same injection molding process conditions, and equivalent molded part performance and properties. Molded parts offer excellent clarity, good toughness, good stiffness, and high surface gloss.

Applications: Major applications include molded boxes and containers, toys, displays, medical devices, overcaps, and novelties.

Processing Recommendations:
Injection Molding: Minimum melt temperature between 193-232°C necessary to permit mold fill. Minimum injection pressure required to fill the cavity. Maximum back pressure of 0.3 MPa. Drying: Generally, no need to dry resin.

Specification Data: FDA Regulation 21 CFR 177.1640. Suitable for contact with non-fatty foods. [Parts over 0.200 inches thick, for alcoholic beverages, or for high temperature food use (hot filled over 150°F or heat sterilized over 212°F) would require additional testing.

Data provided by Chevron Phillips Chemical Company LP.

Available Properties
  • Density
  • Water Absorption
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Impact Test
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Transmission, Visible
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。