Chevron Phillips K-Resin® KR05NW Styrene-Butadiene Copolymer, Sheet and Blow Mold Grade
Subcategory: Styrene-Butadiene; Thermoplastic
Key Words: SBC Poly(Styrene Butadiene)
Material Notes: Styrene-Butadiene Copolymer. No wax (NW) form of K-Resin® KR05 to facilitate printing. Customer Benefits: This SBC is easily processed on blow molding or extrusion and thermoforming equipment. Finished products have excellent clarity, good toughness, good stiffness, high surface gloss, good formability. KR05NW is the no wax form of KR05 to facilitate printing and decorating. Applications: Major applications include bottles, profiles, displays, containers, and unblended sheet. Processing Recommendations: Sheet Extrusion: Melt Temperature, 218°C maximum. High shear and restrictive type screws tend to degrade the melt. Generally no need to dry resin. Blow Molding: 188-196°C for maximum melt strength. Generally no need to dry resin. Injection Blow Molding: Melt Temperature, 232°C maximum. Generally no need to dry resin. Specification Data: FDA Regulation 21 CFR 177.1640. Suitable for food contact. EEC Directive 90/128/EEC and all its amendments. USP Class VI-50. UL 94HB. Data provided by Chevron Phillips Chemical Company LP.
| Available Properties |
- Density
- Water Absorption
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Impact Test
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Transmission, Visible
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|