Chevron Phillips Marlex® K203 Low density, linear hexene copolymer
Subcategory: Polyethylene; Thermoplastic; LLDPE
Key Words: LLDPE
Material Notes: Benefits: good processability, excellent melt strength, excellent flexibility, outstanding stress cracking resistance Characteristics: Bottle ESCR > 700 h, 8-13 cm sheet sag Applications: landfill covers and caps, geomembrane applications, coextruded or blended sheet for thermoformed parts Information provided by Chevron Phillips Chemical Company
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Processing Temperature
|
|
|
|