Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Key Words: UHMWPE
Material Notes: Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistance Characteristics: ESCR > 700 at Condition A, at 50°C; ASTM D 1693 Applications: 55-gallon drums, industrial tanks Information provided by Chevron Phillips Chemical Company