Chevron Phillips Marlex® HHM TR-400G Medium density hexene copolymer
Subcategory: Polyethylene; Thermoplastic; MDPE
Key Words: MDPE
Material Notes: Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistance Applications: pond liners, gas and chemical tank containment liners, landfill liners Information provided by Chevron Phillips Chemical Company
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Processing Temperature
|
|
|
|