Chevron Phillips Marlex® HHM TR-480Z/M362 Natural high density ethylene hexene copolymer/black concrete
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Benefits: good long term hoop strength performance, very high melt strength, outstanding toughness even at low temperatures, concrete base resin Characteristics: Pipe Ring ESCR > 2000 h, ASTM F 1248; 11 Mpa Hydrostatic Design Basis at 23°C and 5.5 Mpa Hydrostatic Design Basis at 60°C Applications: potable water, industrial and mining, oil and gas gathering PENT is 150 hours per ASTM F 1473. Information provided by Chevron Phillips Chemical Company
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Brittleness Temperature
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|