Chevron Phillips Marlex® CL-200YB (Black) Rotational molding crosslinkable high density polyethylene

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Material Notes:
Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, excellent stress cracking resistance to gasoline and other chemicals, outstanding impact strength at temperatures as low as -40°C

Characteristics: 95 J at 3 mm Impact Strength (-40°C); ARM Test Method, 260 J at 6 mm Impact Strength (-40°C); ARM Test Method

Applications: trash containers and lids for automated refuse collection systems, industrial and agricultural chemical storage tanks, small engine, snowmobile, and marine fuel tanks, tractor fuel tanks

Information provided by Chevron Phillips Chemical Company

Available Properties
  • Density
  • Environmental Stress Crack Resistance
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Vicat Softening Point
  • Brittleness Temperature
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。