Chevron Phillips Marlex® CL-200YB (Black) Rotational molding crosslinkable high density polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Benefits: crosslinks during molding - has outstanding melt strength at 204°C, is formulated to provide maximum UV protection for long-term outdoor weathering, contains an internal mold release, excellent stress cracking resistance to gasoline and other chemicals, outstanding impact strength at temperatures as low as -40°C Characteristics: 95 J at 3 mm Impact Strength (-40°C); ARM Test Method, 260 J at 6 mm Impact Strength (-40°C); ARM Test Method Applications: trash containers and lids for automated refuse collection systems, industrial and agricultural chemical storage tanks, small engine, snowmobile, and marine fuel tanks, tractor fuel tanks Information provided by Chevron Phillips Chemical Company
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Brittleness Temperature
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|