Chevron Phillips Marlex® M249 LLDPE Carbon Black Concentrate
Subcategory: Polyethylene; Thermoplastic; LLDPE
Key Words: Linear Low Density Polyethylene
Material Notes:
Processing: to achieve 2.5% carbon black level, the correct let down ratio is 13:1 Information provided by Chevron Phillips Chemical Company.
|
|
|